The product implements the performance requirements of EPDM rubber in the national standard GB/T7594-87, and is applicable to the insulation layer of ordinary rubber cable, mining cable, UCPJB, UCPJR, wind energy cable, etc. Its mechanical and electrical properties are as follows table:
Pilot projects | unit | YXJ-10A | YXJ-30A | YXJ-30A(high pressure) |
standard requirement | Typical value | standard requirement | Typical value | standard requirement | Typical value |
Tensile Strength | N/mm2 | ≥5.0 | 7.0 | ≥5.0 | 8.6 | ≥4.2 | 9.5 |
Elongation at break | % | ≥250 | 280 | ≥250 | 290 | ≥200 | 240 |
Air box heat aging | condition | 5±2℃×240h | 80±2℃×240h | 135±2℃×168h |
Tensile strength change rate | % | ≤±30 | -10.8 | ±30 | -10.1 | ±30 | +0.5 |
Rate of change in elongation at break | % | ≤±30 | -8 | ±30 | -10.2 | ±30 | -14.8 |
Thermal extension test | condition | 250±3℃×15min×0.2Mpa |
Elongation under load | % | ≤100 | 60 | ≤175 | 60 | ≤175 | 65 |
Permanent deformation after cooling | % | ≤25 | 17 | ≤15 | 13 | ≤15 | 13 |
20 ° C volume resistivity | Ω.cm | ≥1.0×1013 | 6.0×1014 | ≥1.0×1014 | 2×1015 | ≥1.0×1015 | 5×1015 |
Dielectric strength | MV/m | 26 | 28 | 28 |
Ozone resistance | condition | 25±2℃×24h×0.025~0.03% |
result | | | | | No crack | No crack |
EPDM insulation rubber 2019-8-30 本文被閱讀 2636 次